Parameter | Description | Example/Unit |
Material Grade | ASTM/AISI/EN standard grade | 304, 316L, 201, 430, 2205 |
Type | Equal Angle / Unequal Angle | 25×25×3mm (Equal) / 40×20×4mm (Unequal) |
Leg Length (A×B) | Length of two legs (equal or unequal) | 20×20mm – 150×150mm (or 1"×1" – 6"×6") |
Thickness (t) | Thickness of angle legs | 1.5mm – 20mm (or 1/16" – 3/4") |
Length | Standard or custom cut length | 6m (20ft), 12m (40ft), Random |
Surface Finish | Surface treatment | Mill Finish, Polished, Brushed |
Tensile Strength | Maximum stress before breaking | 515 MPa (304) / 620 MPa (Duplex) |
Yield Strength | Stress at 0.2% offset deformation | 205 MPa (304) / 450 MPa (Duplex) |
Elongation | Ductility (% elongation at break) | 40% (304) / 25% (Duplex) |
Hardness | Hardness scale (Brinell/Rockwell) | HB ≤ 201 (304) / HB 290 (Duplex) |
Corrosion Resistance | Pitting Resistance Equivalent Number (PREN) | PREN ≥ 18 (316L) / ≥35 (Duplex) |
Tolerance | Leg length/thickness precision | ±1% (Standard) / ±0.5% (Precision) |
Standards | Compliance with international standards | ASTM A554, EN 10088, JIS G4303 |
Certification | Quality/testing certificates | ISO 9001, CE, RoHS |